Through-Hole Soldering That Lasts: the short answer
A good solder joint is made by heating the pad and the component lead together, then feeding solder into the joint, not onto the iron tip. Set a temperature-controlled iron to about 330 to 350 °C for 60/40 tin-lead solder (which melts at about 183 to 190 °C) or about 350 to 380 °C for lead-free SAC305 (about 217 °C).
- Level
- Intermediate
- Time
- About 6 min
- Topic
- Tools and measurement
Make reliable through-hole joints, recognise bad ones by eye, and fix mistakes with wick and a pump.
Before this: Breadboards and Wiring
A good solder joint is made by heating the pad and the component lead together, then feeding solder into the joint, not onto the iron tip. Set a temperature-controlled iron to about 330 to 350 °C for 60/40 tin-lead solder (which melts at about 183 to 190 °C) or about 350 to 380 °C for lead-free SAC305 (about 217 °C). Clean and tin the tip, touch it to both pad and lead for one to two seconds, feed solder from the other side until it flows around the lead, remove the solder, then the iron. The whole joint takes two to four seconds.
A good joint is shiny (dull grey for lead-free is normal), smooth and concave, shaped like a small volcano that wets both the pad and the lead. A ball of solder sitting on the pad is a cold or unwetted joint: the solder never bonded to the pad. A grainy, cracked joint moved while cooling. Too much solder can hide a bridge to the next pad; too little leaves a gap. Trim leads after soldering with flush cutters, and inspect every joint under a magnifier.
Flux does the real work: it removes oxide so solder can wet the metal. The core of the solder wire contains flux, but rework and old parts often need extra flux paste. To remove solder, add fresh solder first (it helps heat flow), then use a desoldering pump or copper wick with flux. Work in a ventilated area, never breathe the flux smoke, wash your hands after handling leaded solder, and always put the iron back in its stand.
Heat the joint, not the solder
A good joint forms when the pad and the lead are both hot enough for the solder to flow onto them. Touch the iron to both for a second or two, feed solder to the joint rather than to the iron tip, then remove the solder and the iron. A good joint is shiny and shaped like a small cone, with solder wetted onto both surfaces.
A dull, grainy or ball-shaped joint is usually a cold joint where the parts were moved or not heated enough. Reheat it with a little fresh solder, or remove it and start again.
Tools and habits
A temperature-controlled iron at about 330 to 350 °C suits leaded solder, and the tip should be clean and tinned. Wipe the tip on a damp sponge or brass wool, and add a little solder to protect it when you put the iron down. Use flux when a joint will not take solder.
Hold the work firmly, with the board flat and the part pressed down before you solder one lead. Check the first lead, then do the rest. Trim the leads after soldering, and wear eye protection when you do.
Safety
Solder in a ventilated space, because flux smoke irritates the lungs. Keep the iron in its stand, wash your hands after handling leaded solder, and never leave a hot iron unattended.
- Melting solder on the iron tip and dabbing it on, so the joint stays cold.
- Moving the part while the solder cools.
- Leaving a hot iron out of its stand.